Hot deformation behaviour of Ti–8Al–1Mo–1V alloy (Ti-811) was investigated through the hot compression tests at the temperatures of 950–1075 °C and at strain rates of 0.001–1 s−1. The flow curves of the Ti-811 alloy were successfully modelled by means of the sinh equation and constitutive equations were proposed for isothermal hot compression of Ti-811 alloy. According to the date of flow curves, the values were calculated for the strain rate sensitivity, stress exponent and activation energy. The amounts of the strain rate sensitivity, stress exponent, and activation energy were calculated as 0.19, 3.95 and 730 kJ mol−1 for α + β region and 0.21, 3.6 and 194 kJ mol−1 for β region, respectively.
Keywords
, Ti–8Al–1Mo–1V alloy, hot deformation behaviour, mechanical analysis, work softening@article{paperid:1097363,
author = {Ebrahimi, GHolam Reza and فاطمه زرقانی and حمید رضا عزت پور and جواد طاهری},
title = {Hot working behaviour of Ti–8Al–1Mo–1V alloy through the hot compression test},
journal = {Materials Science and Technology},
year = {2024},
volume = {40},
number = {10},
month = {July},
issn = {0267-0836},
pages = {755--765},
numpages = {10},
keywords = {Ti–8Al–1Mo–1V alloy; hot deformation behaviour; mechanical analysis; work softening},
}
%0 Journal Article
%T Hot working behaviour of Ti–8Al–1Mo–1V alloy through the hot compression test
%A Ebrahimi, GHolam Reza
%A فاطمه زرقانی
%A حمید رضا عزت پور
%A جواد طاهری
%J Materials Science and Technology
%@ 0267-0836
%D 2024